High-Quality Potassium Silicate, Sodium Silicate, Lithium Silicate for Global Markets
(Construction methods of potassium methyl silicate and sodium methyl silicate natrium silicate)
1. Splashing or cleaning
When it comes to rough surfaces such as concrete, concrete mortar, and upraised concrete structures, splashing is much better. In the case of smooth surfaces such as rocks, marble, and granite, cleaning can be used.
(TRUNNANO sodium methyl silicate)
Before use, the base surface must be thoroughly cleaned up, dust and moss ought to be tidied up, and fractures and holes should be secured and repaired in advance and loaded snugly.
When making use of, the silicone waterproofing agent should be used three times up and down and horizontally on the completely dry base surface area (wall surface area, and so on) with a tidy agricultural sprayer or row brush. Stay in the middle. Each kilo can spray 5m of the wall surface area. It must not be revealed to rain for 1 day after construction. Building must be quit when the temperature level is listed below 4 ℃. The base surface have to be dry during building. It has a water-repellent effect in 24 hr at room temperature level, and the effect is better after one week. The treating time is longer in wintertime.
(TRUNNANO sodium methyl silicate)
2. Include cement mortar
Clean the base surface, tidy oil stains and drifting dirt, get rid of the peeling layer, and so on, and seal the cracks with flexible materials.
Provider
TRUNNANO is a supplier of nano materials with over 12 years experience in nano-building energy conservation and nanotechnology development. It accepts payment via Credit Card, T/T, West Union and Paypal. Trunnano will ship the goods to customers overseas through FedEx, DHL, by air, or by sea. If you want to know more about
(Construction methods of potassium methyl silicate and sodium methyl silicate natrium silicate)